Ụgwọ nke ụlọ ọrụ Hangnie Super Alloys Co., Ltd.
Hangnie Super Alloys Co., Ltd dị na Guxi Town Industrial Park, Taixing City, n'akụkụ osimiri Yangtze. Ọ na-eche Changzhou, Wuxi, na Zhangjiagang ihu n'ofe osimiri ahụ. Ụzọ ụgbọ oloko dị elu nke Shanghai-Chongqing-Chengdu na ọdụ ụgbọ okporo ígwè Xinchang Huangqiao dị ihe dị ka nkeji iri abụọ na oge na ohere. Ejikọtara Gumagan n'Oké Osimiri Yellow dị n'ebe ọwụwa anyanwụ site na mmiri, yana ọdụ ụgbọ mmiri Taizhou dị na ọdịda anyanwụ ruo Osimiri Yangtze - ọdụ ụgbọ mmiri mepere emepe nke mba mbụ. Mpaghara ọnọdụ dị elu na njem mmiri na ala dị mma.
Iji zaghachi nke ọma na "atụmatụ afọ ise nke iri na atọ" ịzụlite na ịzụlite ụlọ ọrụ na-emepụta atụmatụ na atụmatụ "Mere in China 2025", Hangjie Special Alloys (Jiangsu) Co., Ltd. tụpụtara atụmatụ "nzọụkwụ atọ" n'ihi na-ewu nke China si n'ichepụta ike ruo iri afọ atọ, na-arụsi ọrụ ike n'usoro ịzụlite elu-ọgwụgwụ ngwá ọrụ mmepụta na ọhụrụ ihe na-akwalite elu-tech ọrụ na-ike na ibu. Ụlọ ọrụ ahụ goro ndị injinia na-agbaze site na ngalaba na-agbaze nke Shanghai Iron na Steel Research Institute iji mepụta otu nyocha sayensị na nkà na ụzụ na mmepe iji mee ka mmezu nke mmepụta mmepụta ihe ma gbanwee uru nkà na ụzụ n'ime uru mmepụta na uru ahịa, na-eji ezigbo ọrụ na ahụmahụ mmepụta ihe. imepụta ọkachamara: ikuku ikuku, mmanụ ala, petrochemical, elektrọn, ụlọ ọrụ ike nuklia, ụlọ ọrụ kemịkalụ, ụlọ ọrụ mmiri na mpaghara nrụpụta igwe ndị ọzọ na ngwaahịa alloy pụrụ iche na gburugburu ebe ọrụ siri ike.
Hangnie Super Alloys anyị bụ ọkachamara na ịnye Nickel Alloys na igwe anaghị agba nchara n'ọtụtụ ụdị ngwaahịa gụnyere:
Mpempe akwụkwọ, efere, mmanya, ịwụ, TUBE, ọkpọkọ na ihe ndozi.
Anyị nwere ọtụtụ ihe anyị na-akwakọba ma na-ebunye na obere oge nnyefe n'ụwa niile gụnyere:
NICKEL alloy, igwe anaghị agba nchara, DUPLEX, SUPER DUPLEX
Omenala ụlọọrụ
Site na mmepe ngwa ngwa nke ọha mmadụ taa, ụlọ ọrụ ahụ, dị ka mgbe niile, na-agbaso nkà ihe ọmụma azụmahịa nke "àgwà mbụ, iguzosi ike n'ezi ihe mbụ", na-agbalịsi ike maka nlanarị dabere na àgwà, mmepe dabere na aha, ndị ahịa hiwere isi, ahịa-gbakwasara, na-aga n'ihu mmepe na ihe ọhụrụ, na-agbalịsi ike ịkwanye ụlọ ọrụ ahụ n'ọkwa dị elu.
N'otu oge ahụ, na mmụọ nke "ịdị ndụ lanarị, ọhụrụ mmepe", anyị na-agbalịsi ike na-agbalịsi ike maka mma na ihe ọ bụla zuru ezu, ọbọ a mmeri-emeri ọnọdụ ma ụlọ ọrụ mmasị na ahịa mmasị. Ụlọ ọrụ ahụ na-agba mbọ na-ewu ụlọ ọrụ nchekwa akụ na gburugburu ebe obibi nke oge a, ma na-agba mbọ wulite ọkwa ụwa, nyocha dị elu na mmepe na mmepụta ihe maka igwe anaghị agba nchara na ihe alloy pụrụ iche, na-aghọ nhọrọ mbụ maka ndị ahịa.
Ngwaahịa anyị
Ụlọ ọrụ ahụ nwere isi obodo edebanyere aha nke nde yuan 10, na-ekpuchi mpaghara 13,500m2, nwere ụlọ ọrụ nhazi 4 nke nwere ebe a na-arụ ọrụ nke 8,800m2, ma nwee ogbako mgbaze na nkedo na ụlọ ọrụ nhazi ígwè. Companylọ ọrụ ahụ nwere igwe ọkụ dị n'etiti, igwe na-ekpo ọkụ na-ekpo ọkụ, ọkụ induction na-agbaze ọkụ, na ọkụ ọkụ ọkụ electroslag, nwere ikike nrụpụta nke tọn 15,000 kwa afọ, ma gafere nyocha nchekwa na nchekwa gburugburu ebe obibi. Akụrụngwa nyocha nke ọma gụnyere spectrometer, carbon-sulfur analyzer, ultrasonic inspection, tensile test machine, hardness test equipment, etc.
Ụlọ ọrụ ahụ na-emepụta ihe ndị na-emepụta ihe dị elu dị elu dị ka alloys okpomọkụ dị elu, alloys na-eguzogide corrosion, na alloys ziri ezi. Nkọwapụta ngwaahịa gụnyere mmanya, efere, ọkpọkọ, flanges na forgings.
Ngwaahịa: Ogwe ndị a na-ekpo ọkụ na-ekpo ọkụ, Ogwe okirikiri a rụrụ arụ, Ogwe na-egbuke egbuke, akpụ akpụ, ígwè ingots, billlets, ọkpọkọ ígwè, ọkpọkọ flanged, nchara ígwè.
Duplex igwe anaghị agba nchara
F51 (2205 / S31803 / 00Cr22Ni5Mo3N). F52 (S32950). F53(2507 / S32750 / 022Cr25Ni7Mo4N). F55(S32760 / 022Cr25Ni7Mo4WCuN). F60(S32205 /022Cr23Ni5 Mo3N).329 (SUS329J1/ 0Cr26Ni5Mo2/ 1.4460).
Inconel alloy
Inconel600(N06600/ 2.4816).Inconel625(N06625/2.4856).Inconel718(N07718/ 2.4668) Inconel750(N07750).
Incoloy alloy
Incoloy800H (N088100/ 1.4958). Incoloy825 (N08825/ 2.4858). Incoloy925 (N09925) Incoloy926 (N08926/1.4529).
Superalloy
Gr660 (SUH660/ S66286/ A-286/ GH2132/ 0Cr15Ni25Ti2MoAlVB/ 1.4980). Nimonic 80A (N07080/GH4180)
GH3030 (GH30). GH4145 (2.4669). GH4169 (2.4668).
Alloy na-eguzogide corrosion
Nọmba 20 alloy (N08020 / F20). 904 (N08904 / 00Cr20Ni25Mo4.5Cu / 1.4539). 254SMO (F44 / S31254 / 1.4547).
XM-19 (S20910/Nitronic 50).318(3Cr17ni7Mo2N).C4(00Cr14Ni14Si4/ 03Cr14Ni14Si4).
Mmiri ozuzo siri ike igwe anaghị agba nchara
17-4PH (SUS630 / 0Cr17Ni4Cu4Nb). 17-7PH (SUS631 / 0Cr17Ni7Al).
Alloy ego
Monel400 (N04400 / 2.4360 / 2.4361). Monel K-500 (N05500 / 2.4375).
Ngwa nickel alloy
Nickel 200 (N02200/ 2.4060/ 2.4066) .Nickel 201 (N02201/ 2.4061/ 2.4068).
Hastelloy
Hastelloy C (NS333). Hastelloy C-276 (N10276 / 2.4819). Hastelloy C-4 (N06455/ 2.4610). Hastelloy C-22 (N06022).
Hastelloy B (N10001 / 2.4617 / NS321). Hastelloy B-2 (N10665/ 2.4617/ NS322). Hastelloy B-3 (N10675/ 2.4600/ NS323).
Austenitic igwe anaghị agba nchara
F317L (S31703/022Cr19Ni13Mo3). F316Ti (S31635/0Cr18Ni12Mo3Ti/ 06Cr17Ni12Mo2Ti).
310S (S31008/06Cr25Ni20). F347 (S34700/ 06Cr18Ni11Nb). F321 (S32100/0Cr18Ni10Ti/06Cr18Ni11Ti) na ihe ndị ọzọ alloy nwere ihe pụrụ iche.