ALLOY 600 ihe onwunwe data

Nkọwa ngwaahịa

Mkpado ngwaahịa

Akwụkwọ akụkọ nka nka

GH4169 ụlọ mmanya

Ụdị ngwaahịa dị: Pipe, tube, mpempe akwụkwọ, warara, efere, gburugburu mmanya, mmanya dị larịị, ngwaahịa na-emepụta ihe, hexagon, waya na ngalaba extruded

NEL alloyEL alloy HX
INCONEL alloy 22

Ngwakọta kemịkalụ % maka Inconel Alloy 600

Nhọpụta UNS

N06600

Inconel Alloy

600

Nickel (tinyere Cobalt)

72 min.

Chromium

14.0 - 17.0

Ígwè

6.00 - 10.00

Carbon

0.15 kacha.

Manganese

1.0 kacha.

sọlfọ

0.015 kacha.

Silikoni

0.50 kacha.

Ọla kọpa

0.50 kacha.

Mara: Enwere ike ịkọwapụta alloys ndị a ka ọ bụrụ ihe mgbochi ka ukwuun'usoro a kapịrị ọnụ.

INCONEL alloy 600 ka ahapụtara dị ka
UNS N06600
Nọmba ọrụ 2.4816.
A kwadoro alloy ahụ n'okpuru koodu mmiri ọkụ na nrụgide nke American Society of Mechanical Engineers. A kwadoro ya n'okpuru Nkebi nke Mbụ (Ndị na-esi ọkụ ọkụ), Nkebi nke Atọ (Ụgbọ mmiri Nuklia), na Nkebi nke Asatọ (Ụgbọ mmiri nrụgide). A na-ahụ nrụgide imewe nke anabatara na Nkebi II, Nkebi D. Enyere mkpuchi nke ngalaba I site na Code Case 1827.

Mpempe ọla edo edobere na ngwugwu na ngwugwu n'ụlọ nkwakọba ihe nke ngwaahịa ọla. Mpempe akwụkwọ igwe weathered maka owuwu. Ọkpụkpọ ígwè.
Alloy 2205 Duplex igwe anaghị agba nchara (4)

Mkpanaka, Ogwe, Waya na Azụ ahịa
ASTM B 166/ASME SB 166, ASTM B 564/ASME SB 564, ASME Code Cases 1827 na N-253, SAE/AMS 5665 na 5687, BS 3075NA14 na 3076NA14, DIN 177752, 3 , na 9725, MIL-DTL-23229, QQ-W-390.

Efere, Mpempe akwụkwọ na warara
ASTM B 168/ASME SB 168, ASTM B 906/ASME SB 906, ASME Code Cases 1827 na N-253, SAE/AMS 5540, BS 3072NA14 na 3073NA14, DIN 17750, ISO 620IL-2,3M-2508D

Ọkụ na tube
ASTM B 167 / ASME SB 167, ASTM B 163 / ASME SB 163, ASTM B516 / ASME SB 516, ASTM B 517 / ASME SB 517, ASTM B 751 / ASME SB 751, ASTM B 775 / ASME SB 7 /ASME SB 829, ASME.

Usoro koodu1827, N-20, N-253, na N-576, SAE/AMS 5580, DIN 17751, ISO 6207, MIL-DTL-23227.

Ndị ọzọ- ASTM B 366/ASME SB 366, DIN 17742, ISO 4955A, AFNOR NC15Fe