◆ Haynes-188 nwere elu elu okpomọkụ ike, ezigbo mgbochi ọxịdashọn na mgbochi corrosion Njirimara, ọtụtụ-eji na ikuku, petrochemical, shipbuilding na ndị ọzọ ubi.
Ngwakọta kemịkalụ
Ọkwa | C | Si | Mn | S | P | Cr | Ni | Fe | B | Co | W | La | ọzọ |
ọ dịghị ukwuu karịa | |||||||||||||
Haynes-188 | 0.05 ~ 0.15 | 0.2 ~ 0.5 | 1.25 | 0.015 | 0.02 | 21-23 | 20-24 | ≤3 | ≤0.015 | 40–45 | 13–15 | 0.03 ~ 0.15 | - |