Incoloy
Alloy okpomọkụ dị elu
◆Incoloy800H (Ns112 / N08810), Incoloy800HT, Incoloy800 (Ns111 / N08800) bụ atọ ngwaahịa nke otu nickel-ígwè-chromium alloy usoro, ha nwere ezi corrosion eguzogide, creep iguzogide na elu okpomọkụ oxidation iguzogide, ha na-eji na ọxịdashọn na-eguzogide, ha na-eji. ọgwụgwọ Akụrụngwa nwụnye, ngwaọrụ mkpuchi maka mgbochi alloy tubular kpo oku, kemịkalụ na mmanụ mmanụ.
◆Incoloy825 (Ns142/N08825) bụ ihe injinia n'ozuzu. Ọ nwere mgbochi acid na alkali metal corrosion eguzogide ma oxidizing na mbenata gburugburu. Ọdịnaya nickel dị elu na-eme ka alloy nwee nguzogide corrosion nrụgide dị irè. A na-eji ya n'ọtụtụ ebe na mpaghara mmepụta ihe dị iche iche ebe okpomọkụ na-arụ ọrụ adịghị agafe 550 Celsius.
◆Incoloy901 bụ mmiri ozuzo siri ike, ígwè na-eguzogide okpomọkụ. Alloy nwere nnukwu mkpụrụ ike na ike na-adịgide adịgide n'okpuru 650 ° C, ezigbo nguzogide oxidation n'okpuru 760 Celsius, ma kwụsie ike maka iji ogologo oge. A na-eji ya eme ihe n'ọtụtụ ebe n'ichepụta akụkụ dị ka akụkụ ntụgharị nke ụgbọ elu na igwe ikuku gas na-arụ ọrụ n'okpuru 650 Celsius.
◆Incoloy925 (N09925) bụ ihe alloy ígwè na ezi n'ibu ike na nnukwu corrosion eguzogide. A na-ejikarị ya emepụta akụkụ na mmanụ na gas na-egwupụta #equipment.
◆Incoloy926 bụ igwe anaghị agba nchara austenitic nwere ihe mejupụtara kemịkalụ yiri ya na alloy 904L, ọdịnaya nitrogen ya na-abawanye ruo ihe dịka 0.2%, ọdịnaya molybdenum bụ 6.5%. A na-ejikarị ya na injinia mmiri, gburugburu acid gas, flue gas desulfurization system.
◆Incoloy20 bụ ụdị metal ihe nwere ike na-arụ ọrụ ruo ogologo oge n'okpuru elu okpomọkụ n'okpuru 600 ℃ na ụfọdụ nchegbu.
◆Incoloy330 nwere nnukwu ike, ezigbo oxidation eguzogide, corrosion eguzogide, ezi ike ọgwụgwụ na-eguzogide, fracture siri ike na ndị ọzọ Njirimara, na adabara maka nuklia ike, chemical ụlọ ọrụ, na ndị ọzọ n'ibu ubi.
Ngwakọta kemịkalụ
Ọkwa | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | ọzọ |
ọ dịghị ukwuu karịa | |||||||||||||
Incoloy800 | 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | isi | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
Incoloy800H | 0.05 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | isi | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | - |
Incoloy800HT | 0.06 ~ 0.1 | 1 | 1.5 | 0.015 | 0.03 | 19-23 | 30-35 | isi | 0.15 ~ 0.6 | 0.15 ~ 0.6 | ≤0.75 | - | Al + Ti 0.85 ~ 1.2 |
Incoloy825 | 0.05 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ruo 23.5 | 38-46 | isi | ≤0.2 | 0.6 ruo 1.2 | 1.5–3 | 2.5 ruo 3.5 | - |
Incoloy901 | 0.1 | 0.6 | 1 | 0.03 | 0.3 | 11–14 | 40–45 | isi | ≤0.35 | 2.35 ~ 3.1 | ≤0.5 | 5–7 | Co≤1.0 |
Incoloy925 | 0.03 | 0.5 | 1 | 0.03 | 0.03 | 19.5 ruo 23.5 | 42–46 | isi | 0.15 ~ 0.5 | 1.9-2.4 | 1.5–3 | 2.5 ruo 3.5 | - |
Incoloy926 | 0.02 | 0.5 | 2 | 0.01 | 0.03 | 19-21 | 24–26 | isi | - | - | 0.5 ruo 1.5 | 6–7 | N15~0.25 |
Incoloy020 | 0.1 | 0.8 | 0.5 | 0.013 | 0.013 | 23.5 ~ 26.5 | - | 13–16 | ≤1.5 | 0.3 ~ 0.7 | ≤0.5 | 2.5 ruo 3.7 | - |
Incoloy330 | 0.04 ~ 0.08 | 1 nke 1.5 | 2 | 0.03 | 0.03 | 18-20 | 34-37 | isi | - | - | ≤1 | - | - |
Alloy onwunwe kacha nta
Ọkwa | steeti | ike tensile RmN/m㎡ | Mpụta Ike Rp0.2N/m㎡ | Mgbatị dị ka% | Brinell hardness HB |
Incoloy800 | Ọgwụgwọ ọgwụgwọ | 500 | 210 | 35 | - |
Incoloy800H | Ọgwụgwọ ọgwụgwọ | 450 | 180 | 35 | - |
Incoloy800HT | Ọgwụgwọ ọgwụgwọ | 500 | 210 | 35 | - |
Incoloy825 | Ọgwụgwọ ọgwụgwọ | 500 | 220 | 30 | - |
Incoloy901 | Ọgwụgwọ ọgwụgwọ | 900 | 550 | 25 | - |
Incoloy925 | Ọgwụgwọ ọgwụgwọ | 650 | 300 | 30 | - |
Incoloy926 | Ọgwụgwọ ọgwụgwọ | 650 | 295 | 35 | - |
Incoloy20 | Ọgwụgwọ ọgwụgwọ | 700 | 300 | 32 | - |
Incoloy330 | Ọgwụgwọ ọgwụgwọ | 750 | 310 | 35 | - |