MONEL nickel-copper alloy 400 (UNS N04400) bụ ihe ngwọta siri ike nke nwere ike isi ike naanị site na ịrụ ọrụ oyi. Ọ nwere ike dị elu na ike n'elu oke okpomọkụ yana nguzogide dị mma maka ọtụtụ gburugburu ebe obibi. A na-eji Alloy 400 eme ihe n'ọtụtụ ebe, ọkachasị nhazi mmiri na mmiri ọgwụ. Ngwa a na-ahụkarị bụ valvụ na nfuli; mgbapụta mgbapụta na propeller; ihe eji eme mmiri na ihe nkedo; ngwa eletriki na eletriki; isi iyi; akụrụngwa nhazi kemịkalụ; mmanụ ụgbọala na tankị mmiri ọhụrụ; crude petroleum stills, nhazi arịa na ọkpọkọ; ihe ọkụkụ na-eri nri mmiri na-ekpo ọkụ na ihe ndị ọzọ na-ekpo ọkụ; na ndị na-ekpo ọkụ deaerating.Chemical Compositions