Nickel

Nkọwa ngwaahịa

Mkpado ngwaahịa

Alloy okpomọkụ dị elu

◆Nickel200 bụ azụmahịa dị ọcha (99.6%) mere nke nickel, nke nwere ihe ndị dị mma na-arụ ọrụ na ihe ndị dị mma na-eguzogide corrosion, elu okpomọkụ na eletriki eletrik, ọdịnaya gas dị ala na nrụgide dị ala.

◆Nickel201 (N02201) bụ nickel azụmahịa dị ọcha nwere ọdịnaya carbon dị ala, akwadoro ya ka ọ na-eje ozi gburugburu ruo 1230 ℃.

Ngwakọta kemịkalụ

Ọkwa

Ni

Fe

Cu

C

Mn

S

Si

Nickel 200

99

≤0.4

≤0.25

≤0.15

≤0.35

≤0.01

≤0.35

Nickel 201

99

≤0.4

≤0.25

≤0.02

≤0.35

≤0.01

≤0.35

Alloy onwunwe kacha nta

ụdị ngwaahịa

ọnọdụ

ike tensile RmN/m㎡

Mpụta Ike Rp0.2N/m㎡

Mgbatị dị ka%

Brinell hardness HB

osisi na warara

na-ekpo ọkụ akpọrepu

60–85

15–45

35–55

45–80

osisi na warara

oyi adọtara ma ọ bụ annealed

55–75

15-30

40–55

45-70

efere

annealing

55–80

15–40

40 ~ 60

45–75

flakes

annealing

55–75

15-30

40–55

70 Kachasị elu

Ọkụ ígwè

enweghị nkebi annealing

55–75

12-30

40 ~ 60

70 Kachasị elu