  • Nitronic

    Ihe mejupụtara kemịkalụ dị elu Grade C Si Mn SP Cr Ni Fe Mo Ti Cu Nb N ọzọ karịa Nitronic50 0.06 1 4~6 0.03 0.04 20.5~23.5 11.5~13.5 base 1.5~3- 60 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 base — — — — 0.08~0.18 - Alloy onwunwe kacha nta ọkwa ọkwa steeti tensile ike RmN/m㎡ Mpụta Ike Rp0.2N/m ㎡
  • Mpempe akwụkwọ data ihe onwunwe 17-4PH

    Ihe nchọpụta mba ụwa

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Alloy nke ziri ezi

    High Temperature Alloy Chemical compound Grade C Si Mn SP Cr Ni Mo Cu Fe Al Co Ti No greater than 1J50 0.03 0.15~0.3 0.3~0.6 0.02 0.02 - 49.5~50.5 - ≤0.1J3 — 0.5 1.1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 isi — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2~5.8 41.5~ 5.8 41.5~43 0.3 .7 4J29 0,03 0,3 0,5 0,02 0,02 ...
  • nikel

    High Temperature Alloy Chemical composition Grade Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.0.25 ≤0.35 Alloy onwunwe kacha nta ngwaahịa ụdị ọnọdụ tensile ike RmN /m㎡ Ike Mpụta Rp0.2N/m㎡ elongation As% Brinell hardness HB stick and strip hot rolled 60~85 15~45 35~55 45~80 osisi na warara oyi sere ma ọ bụ annealed 55~75 15...
  • Igwe anaghị agba nchara Biphase

    Ihe mejupụtara kemịkalụ dị elu Grade C Si Mn SP Cr Ni Mo Cu NW ọzọ karịa F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - F30 26 6 ~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.3 0.0.0.1 0.5 .035 23–28 3–6 1 3 - - - - A4 ...