Ego 400 Uns N04400 W.Nr.2.4360 na 2.4361
Ngwakọta kemịkalụ
Alloy | mmewere | C | Si | Mn | S | Ni | Fe | Cu |
Ego 400 | Min | 63.0 | 28.0 | |||||
Oke | 0.3 | 0.5 | 2.0 | 0.024 | 2.5 | 34.0 |
Ihe eji arụ ọrụ
Ọnọdụ Aolly | Ike ọdụdọ Rm Mpa Min | Mpụta ike RP 0.2 Mpa Min | Ogologo oge 5% Min |
Ngwọta | 745 | 325 | 40 |
Njirimara anụ ahụ
Ọnọdụ Aolly | Ike tensile Rm Mpa Min. | Ike mpụta RP 0. 2 Mpa Min. | Mgbatị A 5% |
annealed | 480 | 170 | 35 |
Ọkọlọtọ
Mkpanaka, Ogwe, Waya na Azụ ahịaASTM B 164 (Rod, Bar na Waya), ASTM B 564 (Forgings)
Efere, Mpempe akwụkwọ na warara-, ASTM B 127, ASME SB 127
Ọkụ & tubeASTM B165 (Pipu na-enweghị nkebi), ASTM B725 (Welded Pipe), ASTM B730 (Welded Tube), ASTM B 751 (Welded Tube), ASTM B 775 (Welded Pipe), ASTM B 829 (Welded Pipe) Tube)
Ngwaahịa ịgbado ọkụ- Filler Metal 60-AWS A5.14/ERNiCu-7; Welding Electrode 190-AWS A5.11/ENiCu-7.
Njirimara nke Monel 400
● Na-eguzogide mmiri mmiri na uzuoku na oke okpomọkụ
● Nnukwu iguzogide mmiri brackish ma ọ bụ mmiri oké osimiri na-asọ ọsọ ọsọ
● Nguzogide dị oke mma maka mgbawa nrụrụ nrụrụ n'ọtụtụ mmiri dị ọhụrụ
● Ndị na-eguzogide ọgwụ hydrochloric na hydrofluoric acid mgbe ikuku na-ekpochapụ ha
● Na-enye ụfọdụ iguzogide hydrochloric na sulfuric acid na obere okpomọkụ na mkpokọta, mana ọ na-adịkarịghị ihe a na-ahọrọ maka acid ndị a.
● Ezigbo iguzogide nnu na-anọpụ iche na nnu alkaline
● Iguzogide chloride na-akpata nchekasị corrosion mgbawa
● Ngwongwo arụrụ arụ dị mma sitere na okpomọkụ dị n'okpuru efu ruo 1020ºF
● Nnukwu iguzogide alkalis