Inconel
Alloy okpomọkụ dị elu
◆Inconel600 (N06600) nwere corrosion eguzogide dị iche iche corrosive media, ọ nwekwara ezi creep mgbawa ike, akwadoro maka na-arụ ọrụ na gburugburu ebe obibi n'okpuru 700 ℃.A na-ejikarị ya eme ihe na mmepụta na iji ọla alkali na-emebi emebi, karịsịa na gburugburu ebe a na-eji sulfide.
◆Arụ ọrụ dị mkpa nke Inconel601 (N06601) bụ na ọ nwere nguzogide oxidation na nguzogide carbonization dị mma mgbe okpomọkụ dị elu dị ka 1180 Celsius C. A na-ejikarị ya eme ihe na nhazi usoro ọgwụgwọ okpomọkụ, akụkụ usoro ikpochapu, na ikuku oxygen.
◆Inconel625 (N06625Ns336) na-egosipụta nguzogide corrosion dị mma n'ọtụtụ mgbasa ozi, yana 625 dị nro annealed ala-carbon alloy 625 na-ejikarị eme ihe na ụlọ ọrụ usoro kemịkalụ, ebe ọ na-akpọtụrụ mmiri mmiri ma na-eguzogide nrụgide dị elu.
◆Inconel725 nwere nguzogide corrosion nrụgide siri ike ma dabara adaba maka ọkpọkọ ọkpọkọ na arịa mmiri.
◆Inconel690 nwere mgbochi ọxịdashọn na mgbochi corrosion Njirimara, na dabara maka petrochemical, metallurgy, nuklia ike, wdg.
Ngwakọta kemịkalụ
Ọkwa | C | Si | Mn | S | P | Cr | Ni | Fe | Al | Ti | Cu | Mo | Nb | ọzọ |
ọ dịghị ukwuu karịa | ||||||||||||||
Inconel600 | 0.15 | 0.5 | 1 | 0.015 | 0.03 | 14-17 | isi | 6–10 | - | - | ≤0.5 | - | - | - |
Inconel601 | 0.1 | 0.5 | 1 | 0.015 | 0.03 | 21-25 | isi | 10–15 | 1 nke 1.7 | - | ≤1 | - | - | - |
Inconel625 | 0.1 | 0.5 | 0.5 | 0.015 | 0.015 | 20-23 | isi | ≤5 | ≤0.4 | ≤0.4 | - | 8-10 | 3.15 ~ 4.15 | Co≤1 |
Inconel725 | 0.03 | 0.2 | 0.35 | 0.01 | 0.015 | 19-22.5 | 55–59 | Nọgidenụ | 0.35 | 1 nke 1.7 | - | 7-9.5 | 2.75 ~ 4 | - |
Njikọ 690 | 0.05 | 0.5 | 0.5 | 0.015 | 0.03 | 27-31 | ≥58 | 7-11 | - | - | ≤0.5 | - | - | - |
Alloy onwunwe kacha nta
Ọkwa | alloy steeti | ike tensile RmN/m㎡ | Mpụta Ike Rp0.2N/m㎡ | Mgbatị dị ka% | Brinell hardness HB |
Inconel600 | Ọgwụgwọ ọgwụgwọ | 550 | 240 | - | ≤195 |
Ọgwụgwọ ọgwụgwọ | 500 | 180 | - | ≤185 | |
Inconel601 | Na-ewe iwe | 650 | 300 | - | - |
Ọgwụgwọ ọgwụgwọ | 600 | 240 | - | ≤220 | |
Inconel625 | Ọgwụgwọ ọgwụgwọ | 760 | 345 | - | ≤220 |
Inconel725 | Ọgwụgwọ ọgwụgwọ | 790 | 485 | 28 | - |
Njikọ 690 | Ọgwụgwọ ọgwụgwọ | 780 | 450 | 25 | - |